Grade NS1402
H08825
Old Grade
Corresponding Standard YB /T 5354-2012
Cold-rolled plates of corrosion-resisting alloys
Classification Special Alloy Steel
NS1402 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti Al More
Minimum Value - - - - - 19.5 38 1.5 2.5 0.6 - Fe:Remanider
Maximum Value 0.05 0.5 1 0.03 0.015 23.5 46 3 3.5 1.2 0.2
* Fe≥22.0% is determined by arithmetic difference.
NS1402 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
solution temperature 940~1050°C ≥586 ≥241 ≥30
Approximate Comparison Table Corrosion-Resistant Alloy
China Japan South Korea United States Germany United Kingdom
GB ISC JIS KS Commercial Grade UNS DIN EN/DIN W-Nr. BS EN/BS
NS 1402
(NS 142)
(0Cr21Ni42Mo3Cu2Ti)
H 08825
H 01402
NCF 825 NCF 825 Incoloy 825 N 08825 NiCr21Mo 2.4858 NA 16

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!