Grade HT350
Corresponding Standard GB /T 9439-2010
Grey Iron Castings
Classification cast Iron
HT350 Mechanical Properties
Sample size Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
φ30 (single-cast) 350~450 228~285 0.3~0.8
10<t≤300 (single-cast) ≥350 220~290
20<t≤40 (additional casting) ≥290
40<t≤80 (additional casting) ≥260
80<t≤150 (additional casting) ≥230
150<t≤300 (additional casting) ≥210
10<t≤20 (base material) ≥315
20<t≤40 (base material) ≥280
40<t≤80 (base material) ≥250
80<t≤150 (base material) ≥225
Approximate Comparison Table Cast Iron
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB JIS ASTM SAE ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
HT350 FC350 50
350
G13H24 350
JL350
GG35 0.6035 FGL350 EN-GJL-350 EN-JL1060 SCH35 0135 350 T350
HT350 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!