Grade 52SiCrNi5
European Standard Steel Grade 1.7117
Corresponding Standard EN 10089-2002
Hot rolled steels for quenched and tempered springs; technical delivery conditions
Classification Spring Steel
Properties Strength Elasticity Fatigue Resistance Quench Hardness
52SiCrNi5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value 0.49 1.2 0.7 - - 0.7 0.5 Cu+10Sn ±0.60
Maximum Value 0.56 1.5 1 0.025 0.025 1 0.7
52SiCrNi5 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, rod +QT 1450~1750 ≥1300 ≥6 ≥35 - KU
≥10
Rod +S - - - - ≤280 -
Bar, rod +A - - - - ≤248 -
Bar, rod +AC - - - - ≤230 -
52SiCrNi5 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!