Grade QT600-3
Corresponding Standard YB /T 036.2-1992
General Technical Conditions for Metallurgical Equipment Manufacturing - Cast Iron Parts
Classification cast Iron
QT600-3 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
QT600-3 (Single Cast) ≥600 ≥370 ≥3 190~270
QT600-3A (Attached Cast), Wall Thickness > 30~60mm ≥600 ≥360 ≥3 180~270
QT600-3A(附铸) , 壁厚>60~200mm ≥550 ≥340 ≥1 180~270
Approximate Comparison Table Cast Iron
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
QT600-3 FCD600
FCD600-3
100-70-03
80-55-06
80-60-03
600-3
600-3/S
600-3/U
GGG60 0.7060 600-3
FGS600-3
EN-GJS-600-3 5.3201
(EN-JS1060)
VCH60 0732-03
32-03
600/3 600-3
QT600-3 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!