Grade HTRSi5
Corresponding Standard GB /T 9437-2009
Heat resistant iron castings
Classification cast Iron
HTRSi5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 2.4 4.5 - - - 0.5
Maximum Value 3.2 5.5 0.8 0.1 0.08 1
HTRSi5 Mechanical Properties
Tensile Strength
σb
Mpa
Hardness
HBW
Room Temperature ≥140 160~270
Short-term high temperature 700°C ≥41
Short-term high temperature 800°C ≥27