Grade GCr15
Corresponding Standard YB /T 4323-2013
Centrifugal casting pipe billet
Classification Bearing Steel
GCr15 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.95 0.15 0.25 - - 1.4 - - -
Maximum Value 1.05 0.35 0.45 0.025 0.025 1.65 0.3 0.25 0.08
1 Approximate Comparison Table High-Carbon Chromium Bearing Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SKF BS EN/BS
GCr15 B00150 SUJ2 SUJ2 STB2 E52100 G52986 100Cr6
(B1)
100Cr6
(W3)
1.3505 100Cr6
(100C6)
ЩХ15 SKF3 535A99
2 Approximate Comparison Table Alloy Cold-Work Tool Steel
China Japan United States Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
Cr2
GCr15
SUJ2 52100 100Cr6 100Cr6
100Cr6RR
102Cr6 1.2067 KH
ShKh15
2258 534A99
535A99
GCr15 Corresponding Standards(Same grade name, different standards)