Grade G20CrNiMoA
Corresponding Standard GB /T 3203-2016
Carburizing Steels for Bearing
Classification Bearing Steel
Properties High Strength High Hardness Impact Resistance Fatigue Resistance
G20CrNiMoA Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Ti Al H Ca
Minimum Value 0.17 0.15 0.6 - - 0.35 0.4 - 0.15 - - - -
Maximum Value 0.23 0.4 0.9 0.02 0.015 0.65 0.7 0.25 0.3 0.005 0.05 0.0002 0.001
G20CrNiMoA Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
d=15* Double Quenching + Oil Cooling, Tempering + Air Cooling ≥1180 ≥9 ≥45 - ≥63
Delivery Condition** WHR+SA/WHF/WHF+SA/WCD/SF or SP - - - ≤229 -

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!