Grade SA-193 Grade B7
Corresponding Standard ASME SA-193/SA-193M-2019
Standard Specification for Alloys-Steel and Stainless Steel Bolting for High-Temperature or or High Pressure Service and Other Special Purpose Applications
Classification Alloy Steel
SA-193 Grade B7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.37 0.15 0.65 - - 0.75 0.15
Maximum Value 0.49 0.35 1.1 0.035 0.04 1.2 0.25
SA-193 Grade B7 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
d≤M64 Tempering Temperature ≥593°C ≥860 ≥720 ≥16 ≥50 ≤321
M64<d≤M100 Tempering Temperature ≥593°C ≥795 ≥655 ≥16 ≥50 ≤321
M100<d≤M180 Tempering Temperature ≥593°C ≥690 ≥515 ≥18 ≥50 ≤321

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!