Grade S82
Other Names
Corresponding Standard BS 5S S82-1976
Specification for 4% nickel-chromium-molybdenum case-hardening steel billets, bars, forgings and parts (1320-1520 MPa)
Classification Alloy Steel
Properties Strength
S82 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.14 0.15 0.25 - - 1 3.8 0.2
Maximum Value 0.18 0.4 0.55 0.025 0.02 1.4 4.3 0.3
S82 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar Stock, Ingot, Forging Heat Treatment 1320~1520 ≥1030 ≥8 ≥35 Izod
≥34
Bar Stock, Ingot, Forging Normalizing and Softening ≤277

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!