Grade 09CuPCrNi-A
Corresponding Standard GB 4171-1984
Superlor antomspheric corrosion resisting structual steel
Classification Alloy Steel
09CuPCrNi-A Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value - 0.25 0.2 0.07 - 0.3 - 0.25
Maximum Value 0.12 0.75 0.5 0.15 0.04 1.25 0.65 0.55
09CuPCrNi-A Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 6 (Hot Rolled) ≥480 ≥343 ≥22
t > 6 (Hot Rolled) ≥480 ≥343 ≥22
t ≤ 2.5 (Cold Rolled) ≥451 ≥314 ≥26
12 ≤ t ≤ 16 (Longitudinal) Temperature 0°C ≥28
New and Old Grade Replacement List
Corresponding Standard Grade
GB 4171-1984
Grade
GB /T 4171-2000
Grade
China ISC
Approximate Comparison Table structural alloy steel
China Japan United States International Organization for Standardization Germany France European Standard United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade BS EN/BS
09CuPCrNi-A SPA-H Gr.1 Fe355W-1A 9CrNiCuP324 E36WA3 S355J0WP
Fe510C1KI①
1.8945 WR50A
WR50B
WR50C
09CuPCrNi-A Corresponding Standards(Same grade name, different standards)