Grade En36A
Corresponding Standard BS 970-1955
Wrought Steels IN THE FORM OF BARS, BILLETS AND FORGINGS UP TO 6 IN. RULING SECTION FOR AUTOMOBILE AND GENERAL ENGINEERING PURPOSE
Classification Alloy Steel
En36A Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo * V *
Minimum Value - 0.1 0.3 - - 0.6 3 - -
Maximum Value 0.15 0.35 0.6 0.05 0.05 1.1 3.75 0.15 0.05
En36A Mechanical Properties
diameter or width across flats
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Bars, forged billets, forgings, mechanical bars, bright bars; d≤28.6 Heat Treatment ≥849 ≥15 ≥47
• d-diameter or width across flats/mm
• The unit conversion for strength is based on: 1tons/sq.in=15.44N/mm2
• The unit conversion for impact energy absorption is based on: 1ft.lb=1.3558J
Approximate Comparison Table structural alloy steel
China United Kingdom
GB BS EN/BS
15CrNi3 EN36A

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!