Grade C5341
Other Names
Corresponding Standard JIS H 3270-2018
Copper beryllium alloy, phosphor bronze and nickle silver rods, bars and wires
Classification Copper and Copper Alloys
C5341 Chemical Element Composition Content (%)
Component P Pb Sn More
Minimum Value 0.03 0.8 3.5 Cu+Sn+P+Pb≥99.5
Maximum Value 0.35 1.5 5.8
C5341 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar (B, BS); 0.5≤d≤3 Hardening treatment (H) ≥470 HV
≥125
Bars (B, BS); 3 < d ≤ 6 Hardening treatment (H) ≥440 ≥125
Bars (B, BS); 6 < d ≤ 13 Hardening treatment (H) ≥410 ≥10 ≥115
Bars (B, BS); 13 < d ≤ 25 Hardening treatment (H) ≥375 ≥12 ≥110
Bars (B, BS); 25 < d ≤ 50 Hardening treatment (H) ≥345 ≥15 ≥100
Bars (B, BS); 50 < d ≤ 100 Hardening treatment (H) ≥320 ≥15 HRBS
60~90
d=diameter or width across flats; unit mm

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!