Grade C7541
Other Names
Corresponding Standard JIS H 3270-2018
Copper beryllium alloy, phosphor bronze and nickle silver rods, bars and wires
Classification Copper and Copper Alloys
C7541 Chemical Element Composition Content (%)
Component Fe Mn Ni Cu Pb More
Minimum Value - - 12.5 60 - Zn:余量
Maximum Value 0.25 0.5 15.5 64 0.03
C7541 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Hardness
HBW
Bar stock (B); 3≤d≤6 1/2 Hard (1/2H) 440~590 HV
≥135
Bar stock (B); 6<d≤13 1/2 Hard (1/2H) 390~540 ≥120
Bar stock (B); 3≤d≤6 Hard (H) 570~705 ≥150
Bar stock (B); 6<d≤13 Hard (H) 520~645 ≥135
Bar (B); 13<d≤25 Hard (H) 450~590 ≥115
Bar (B); 25<d≤50 Hard (H) 390~540 ≥100
wire (W); 0.4 ≤ d ≤ 5 Annealing (O) 365~510
wire (W); 0.4 ≤ d ≤ 5 1/2 Hard (1/2H) 510~665
wire (W); 0.4 ≤ d ≤ 5 Hard (H) ≥635
d=diameter or width across flats; unit mm
Approximate Comparison Table Wrought Cupronickel
China Japan United States International Organization for Standardization Russia United Kingdom
GB ISC JIS ASTM UNS ISO Numerical Grade GOST Commercial Grade BS EN/BS
BZn15-20 T74600 C7541
C75400
63Cu-15Ni-22Zn C75400 CuNi15Zn21 C75400 МНЦ15-20 NS105 C75400
C7541 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!