USA UNS N08800
ASTM
Specification or Grade
800
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu Ti Al
Minimum Value 39.5 - - - - - 19 30 - 0.15 0.15
Maximum Value - 0.1 1 1.5 0.045 0.015 23 35 0.75 0.6 0.6
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Annealing - Hot or Cold Precision Rolling (A) ≥515 ≥205 ≥30 ≤192
1 Approximate Comparison Table corrosion-resistant alloy
China Japan South Korea United States Germany United Kingdom
GB ISC JIS KS Commercial Grade UNS DIN EN/DIN W-Nr. BS EN/BS
NS 1101
(NS 111)
(0Cr20Ni32AlTi)
H 08800
H 01101
NCF 800
(NCF 2B)
NCF 800 Incoloy 800 N 08800 X10NiCrAlTi 32-20 1.4876 NA 15
2 Approximate Comparison Table
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade EN Numerical Grade
NCF800 N08800 X8NiCrAlTi32-21 4876-088-00-1 X8NiCrAlTi32-21 1.4959
1.4876
3 Approximate Comparison Table
United States International Organization for Standardization European Standard
ASTM UNS ISO EN Numerical Grade
800 N08800 X8NiCrAlTi32-21 X10NiCrAlTi32-21 1.4876