USA UNS S20200
ASTM
Specification or Grade
202
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 7.5 - - 17 4 -
Maximum Value 0.15 1 10 0.06 0.03 19 6 0.25
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
all Annealing - Hot or Cold Precision Rolling (A) ≥515 ≥275 ≥40 ≥45
≤19.05 Relatively Strict Cold Working (B) ≥860 ≥690 ≥12 ≥35
>19.05~25.4 Relatively Strict Cold Working (B) ≥795 ≥550 ≥15 ≥35
>25.4~31.75 Relatively Strict Cold Working (B) ≥725 ≥450 ≥20 ≥35
>31.75~38.1 Relatively Strict Cold Working (B) ≥690 ≥345 ≥24 ≥45
>38.1~44.45 Relatively Strict Cold Working (B) ≥655 ≥310 ≥28 ≥45
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS EN Numerical Grade GOST BS EN/BS
12Cr18Mn9Ni5N S35450 202 SUS 202 STS 202 202 S20200 X12CrMnNi 18-9-5 1.4373 12Х17Г9АН4 284S16
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S35450 SUS202 S20200 X12CrMnNiN18-9-5 4373-202-00-I 1.4373

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!