USA UNS S20500
ASTM
Specification or Grade
205
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value 0.12 - 14 - - 16.5 1 0.32
Maximum Value 0.25 1 15.5 0.06 0.03 18 1.7 0.4
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Annealing - Hot or Cold Precision Rolling (A) ≥690 ≥414 ≥40 ≥50