USA UNS S30453
ASTM
Specification or Grade
304LN
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 18 8 0.1
Maximum Value 0.03 1 2 0.045 0.03 20 11 0.16
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
all Annealing - Hot Finish Rolling (A) ≥515 ≥205 ≥40 ≥50
≤12.7 Annealing - Cold Precision Rolling (A) ≥620 ≥310 ≥30 ≥40
>12.7 Annealing - Cold Precision Rolling (A) ≥515 ≥205 ≥30 ≥40
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
022Cr19Ni10N
(00Cr18Ni10N)
S30453 304LN SUS 304LN STS 304LN 304LN S30453 X2CrNiN 18-9
X2CrNiN18-10
X2CrNiN 18-10 1.4311 Z2CN 18-1Az
Z3CN18-10Az
X2CrNiN 18-10 1.4311 2371 304S62
304S61

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!