USA UNS S40976
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Ferritic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N More
Minimum Value - - - - - 10.5 0.75 - Cb:10×(C+N)-0.80
Maximum Value 0.03 1 1 0.04 0.03 11.7 1 0.04
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Annealing - Hot or Cold Precision Rolling (A) ≥415 ≥140 ≥20 ≥45 ≤244
Approximate Comparison Table Ferritic Heat-Resistant Steel
China United States International Organization for Standardization European Standard
GB ISC UNS ISO Numerical Grade EN Numerical Grade
022Cr11NiNbTi
GB/T 20878-2024
S11164 S40976
ASTM A959
X6CrNiTi12
ISO 15510
4516-409-75-Ⅰ X6CrNiTi12 1.4516

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!