USA UNS S41040
ASTM
Specification or Grade
XM-30
Corresponding Standard ASTM A276/A276M-2017
Standard Specification for Stainless Steel Bars and Shapes
Classification Martensitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cb
Minimum Value - - - - - 11 0.05
Maximum Value 0.18 1 1 0.04 0.03 13 0.3
Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Hot rolled Annealing (A) ≥480 ≥275 ≥13 ≥45 ≤235
Cold rolled Annealing (A) ≥480 ≥275 ≥12 ≥35
Hot rolled Quenching and Tempering at Relatively High Temperatures (T) ≥860 ≥690 ≥13 ≥45 ≤302
Cold rolled Quenching and Tempering at Relatively High Temperatures (T) ≥860 ≥690 ≥12 ≥35

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!