USA UNS N06002
Corresponding Standard ASTM B435-2006
Standard Specification for UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip
Classification Alloy Steel
Properties Corrosion Resistance
Density 8.23 g/cm3
Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Mo W Co More
Minimum Value 17 0.05 - - - - 20.5 8 0.2 0.5 Ni:余量
Maximum Value 20 0.15 1 1 0.04 0.03 23 10 1 2.5
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Sheet; t≥4.76 Hot rolling, solution annealing, descaling ≥655 ≥240 ≥35
Thin sheet, strip; t<4.76 Hot rolling or cold rolling, annealing and descaling ≥655 ≥240 ≥35
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany
GB ISC Commercial Grade UNS W-Nr.
NS 3312
GH 3536
H 06002 Hastelloy X N 06002 2.4665
2 Approximate Comparison Table Wrought Corrosion-Resistant Alloy for Welding
China United States International Organization for Standardization
GB ISC UNS ISO
HNS 3312
NiCr21Fe18 Mo9
W 56600 N 06002 SNi 6002