USA UNS S28200
Corresponding Standard ASTM A473-2018
Stainless Steel Forgings
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo N
Minimum Value - - 17 - - 17 0.75 0.75 0.4
Maximum Value 0.15 1 19 0.045 0.03 19 1.25 1.25 0.6
Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
≥760 ≥415 ≥40 ≥50

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!