Grade F 467MAB Cu 260
USA UNS C26000
Corresponding Standard ASTM F467M-2006(R2012)
Nonferrous Nuts for General Use (Metric)
Classification Copper and Copper Alloys
F 467MAB Cu 260 Chemical Element Composition Content (%)
Component Fe Cu Pb More
Minimum Value - 68.5 - Zn余量
Maximum Value 0.05 71.5 0.07
F 467MAB Cu 260 Mechanical Properties
Hardness
HBW
HRF
≥55
1 Approximate Comparison Table Brass
China Japan United States International Organization for Standardization Germany European Standard Russia
GB JIS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. EN Numerical Grade GOST
H70 C2600 70Cu-30Zn C26000 CuZn30 C26000 CuZn30 C26000
2.0265
CuZn30 CW505L Л70
2 Approximate Comparison Table Copper and Copper Alloy
Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
JIS UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
C2600 C26000 CuZn30 CuZn30 2.0265 CuZn30 CuZn30 CW505L L70 CuZn30 CZ106

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!