Grade SNC415
Old Grade
Corresponding Standard JIS G 4102-1979
Nickel chromium steels
Classification Alloy Steel
SNC415 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.12 0.15 0.35 - - 0.2 2 -
Maximum Value 0.18 0.35 0.65 0.03 0.03 0.5 2.5 0.3
SNC415 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Double Quenching and Tempering ≥785 ≥17 ≥45 235~341 ≥88
New and Old Grade Replacement List
Corresponding Standard Grade
JIS G 4102-1979
Grade
Old Grade
JIS G 4053-2003
Grade
JIS G 4053-2016
Grade
Approximate Comparison Table Structural Alloy Steel
China Taiwan, China Japan South Korea United States Germany France Russia
GB ISC CNS JIS KS ASTM/AISI DIN EN/DIN W-Nr. NF EN/NF GOST
12CrNi2 A41122 SNC415 SNC415 SNC415 3415 14NiCr10 1.5732 14NC11 12ХН2А