Grade 06Cr18Ni10Ti
Old Grade
Corresponding Standard GJB 2294A-2014
Specification for stainless and heat-resisting steel bars for aviation
Classification Austenitic Stainless Steel
06Cr18Ni10Ti Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Ti:5C ~ 0.70
Maximum Value 0.08 1 2 0.035 0.02 19 12
06Cr18Ni10Ti Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Quenching or solution treatment 1010~1150°C, water cooling ≥520 ≥205 ≥40 ≥50
06Cr18Ni10Ti Corresponding Standards(Same grade name, different standards)