Grade A600 T8
USA UNS T12008
AISI
American Iron and Steel Institute
T8
Corresponding Standard ASTM A600-1992(R2010)
Standard Specification for Tool Steel High Speed
Classification Alloy Steel
A600 T8 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo W V Co More
Minimum Value 0.75 0.2 0.2 - - 3.75 0.4 13.25 1.8 4.25 Ni+Cu≤ 0.75
Maximum Value 0.85 0.4 0.4 0.03 0.03 4.5 1 14.75 2.4 5.75
A600 T8 Mechanical Properties
Heat Treatment or Condition
Hardness
HBW
Bars, forgings, thick plates, thin plates, strip products Cold Drawing HB
≤293
Bars, forgings, thick plates, thin plates, strip products Cold Drawn and Annealed ≤285
Bars, forgings, thick plates, thin plates, strip products Annealing ≤277
Bars, forgings, thick plates, thin plates, strip products Heat Treatment HR
≥65