Grade Z 7 CND 17-11-02
Other Names
Corresponding Standard NF A 35-573-1996
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Z 7 CND 17-11-02 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 16 10 2
Maximum Value 0.07 1 2 0.04 0.03 18 12 2.5
Z 7 CND 17-11-02 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Plates, Strips, and Wide Strips; t≤5 550~700 ≥240 ≥40
Plates, Strips, and Wide Strips; 5<t≤75 550~700 ≥220 ≥45
Approximate Comparison Table Austenitic Stainless Steel
China Japan United States Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
0Cr17Ni12Mo2 SUS316 316 X5CrNiMo17-12-2 Z6CND17-11
Z7CND17-11-02
Z7CND17-12-02
X5CrNiMo17-12-2 1.4401 08KH16N11M3 2347 316S31