Grade NCF600
Corresponding Standard JIS G 4901-2008
Corrosion-Resistant and Heat-Resisting Superalloy Bars
Classification Alloy Steel
Properties Corrosion Resistance
NCF600 Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Cu
Minimum Value 6 - - - - - 14 72 -
Maximum Value 10 0.15 0.5 1 0.03 0.015 17 - 0.5
NCF600 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar stock; d>2.5 Annealing (A) ≥550 ≥245 ≥30 ≤179
Approximate Comparison Table Corrosion-Resistant Alloy
China Japan South Korea United States Germany United Kingdom
GB ISC JIS KS Commercial Grade UNS W-Nr. L-Nr. BS EN/BS
NS 3102
(NS 312)
(1Crl 5 Ni75Fe8)
H 06600
H 03102
NCF 600 NCF 600 Inconel 600 N 06600 NiCr15Fe 2.4816 NA 14