Grade NCF800H
Corresponding Standard JIS G 4901-2008
Corrosion-Resistant and Heat-Resisting Superalloy Bars
Classification Alloy Steel
Properties Corrosion Resistance
NCF800H Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Ti Al More
Minimum Value 0.05 - - - - 19 30 - 0.15 0.15 Fe:余量
Maximum Value 0.1 1 1.5 0.03 0.015 23 35 0.75 0.6 0.6
NCF800H Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar stock; d>2.5 Solution (S) ≥450 ≥175 ≥30 ≤167
Approximate Comparison Table Austenitic Stainless Steel
Japan United States International Organization for Standardization European Standard
JIS UNS ISO Numerical Grade Numerical Grade
NCF800H N08810 X7NiCrAlTi33-21 4959-088-10-U 1.4959
NCF800H Corresponding Standards(Same grade name, different standards)