Grade NCF80A
Corresponding Standard JIS G 4901-2008
Corrosion-Resistant and Heat-Resisting Superalloy Bars
Classification Alloy Steel
Properties Corrosion Resistance
NCF80A Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Cu Ti Co Al More
Minimum Value - 0.04 - - - - 18 - 1.8 - 1 Ni+Co:余量
Maximum Value 1.5 0.1 1 1 0.03 0.015 21 0.2 2.7 2 1.8
NCF80A Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Bars; 2.5<d≤100 Solution (S) - - - ≤269
Bars; 2.5<d≤100 Solution Heat Treatment + Aging (H) ≥1000 ≥600 ≥20 -
Approximate Comparison Table Deformed High-Temperature Alloy
China Japan United States Germany France Russia United Kingdom
GB JIS SAE W-Nr. L-Nr. NF EN/NF GOST Commercial Grade BS EN/BS
GH80A NCF80A HEV5 2.4952 2.4631 ATGS3
NC20TA
ЭИ445 ANC.9
N80A
DTD736B
HR1
HR201
HR401
HR601
NCF80A Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!