Grade A322 5160
USA UNS G51600
Corresponding Standard ASTM A322-2013(R2018)
Steel Bars, Alloy, Standard Grades
Classification Alloy Steel
A322 5160 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.56 0.15 0.75 - - 0.7 - - -
Maximum Value 0.64 0.35 1 0.035 0.04 0.9 0.25 0.35 0.06
① Silicon may be specified by the purchaser as 0.10 % maximum. The need for 0.10 % maximum generally relates to severely cold-formed parts
② These elements are considered as incidental and may be present to the table maximum amounts.
③ Standard alloy steels can be produced with a lead range of 0.15 to 0.35 %. Such steels are identified by inserting the lette “L” between the second and third numerals of the number, that is, 41 L40. A cast or heat analysis is not determinable when lead is added to the ladle stream
Approximate Comparison Table Spring Steel
China Taiwan, China Japan South Korea United States United Kingdom
GB ISC CNS JIS KS AISI UNS BS EN/BS
60CrMnA A22603 SUP9A SUP9A SPS5A 5160 G51600 527A60