Grade A268 29-4
USA UNS S44700
Corresponding Standard ASTM A268/A268M-2020
Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service
Classification Ferritic Stainless Steel
A268 29-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N More
Minimum Value - - - - - 28 - - 3.5 - C+N≤0.025
Maximum Value 0.01 0.2 0.3 0.025 0.02 30 0.15 0.15 4.2 0.02
A268 29-4 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥550 ≥415 ≥20 ≤207
Approximate Comparison Table Ferritic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S13091 SUS447J1 S44700 X1CrMo30-2 4135-447-92-C (1.4135)
A26829-4 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!