Grade 12CrMo4
European Standard Steel Grade 1.7201
Corresponding Standard EN 10263-3-2017
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion Part 3: Technical Delivery Conditions for Steels for Case Hardening Steels
Classification Alloy Steel
12CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo
Minimum Value 0.1 - 0.6 - - 0.9 - 0.15
Maximum Value 0.15 0.3 0.9 0.025 0.025 1.2 0.25 0.25
12CrMo4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Hardness
HBW
Bars; 5<d≤40 Processed to Ferrite-Pearlite Structure and Hardness Range (+FP) 135~185
Bars; 5<d≤40 Spheroidizing (+AC) ≤500 ≥62
Bar, wire; 2<d≤5 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤500 -
Bar, wire; 5<d≤40 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤480 ≥64
Bar, wire; 5<d≤40 Untreated, Cold Drawn, Spheroidizing Treatment, and Tempered Rolling (+U+C+AC+LC) ≤520 ≥62
Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
12CrMo4 12CrMo4 1.7201
12CrMo4 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!