Grade 16MnCr5
European Standard Steel Grade 1.7131
Corresponding Standard EN 10263-3-2017
Steel rod, bars and wire for cold heading and cold extrusion Part 3: Technical delivery conditions for steels for case hardening steels
Classification Alloy Steel
16MnCr5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.14 - 1 - - 0.8 -
Maximum Value 0.19 0.3 1.3 0.025 0.025 1.1 0.25
16MnCr5 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Hardness
HBW
Bars; 5<d≤40 Processed to Ferrite-Pearlite Structure and Hardness Range (+FP) 140~187
Bars; 5<d≤40 Spheroidizing (+AC) ≤550 ≥62
Bar, wire; 2<d≤5 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤550 ≥64
Bar, wire; 5<d≤40 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤530 ≥64
Bar, wire; 2<d≤5 Untreated, Cold Drawn, Spheroidizing Treatment, and Tempered Rolling (+U+C+AC+LC) ≤590 ≥62
Bar, wire; 5<d≤40 Untreated, Cold Drawn, Spheroidizing Treatment, and Tempered Rolling (+U+C+AC+LC) ≤570 ≥62
Bars, wire; 5<d≤10 Spheroidizing Treatment and Cold Drawing (+AC+C) ≤660 ≥59
Bars, wire; 10<d≤40 Spheroidizing Treatment and Cold Drawing (+AC+C) ≤650 ≥59
1 Approximate Comparison Table Structural Alloy Steel
China International Organization for Standardization European Standard
GB ISO EN Numerical Grade
16CrMnH 16MnCr5 16MnCr5 1.7131
2 Approximate Comparison Table Structural Alloy Steel
China United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB SAE ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
15CrMn
16MnCr
20CrMnTi
5115 16MnCr5 16MnCr5 16MC5 16MnCr5 1.7131 18KHG 2127 527M17
590M17
3 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
China International Organization for Standardization European Standard
GB ISO EN Numerical Grade
16CrMnH 16MnCr5 16MnCr5 1.7131