Grade S355K2
European Standard Steel Grade 1.0596
Corresponding Standard EN 10025-2-2019
Hot rolled products of structural steels - Part 2: Technical delivery conditions for non-alloy structural steels
Brand/Supplier
-> BENSTEEL
-> BAOSTEEL
Classification Carbon Steel
Density 7.85 g/cm3
S355K2 Chemical Element Composition Content (%)
  Component C Si Mn P S Cu
d≤30 Minimum Value - - - - - -
Maximum Value 0.2 0.55 1.6 0.025 0.025 0.55
  Component C Si Mn P S Cu
d>30 Minimum Value - - - - - -
Maximum Value 0.22 0.55 1.6 0.025 0.025 0.55
• FN= rimming steels not permitted; FF = fully killed steel
S355K2 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Long products and flat products; t≤1 510~680 ≥355 ≥14 -20°C
≥40
Long and flat products; 1<t≤1.5 510~680 ≥355 ≥15 ≥40
Long and flat products; 1.5<t≤2 510~680 ≥355 ≥16 ≥40
Long and flat products; 2<t≤2.5 510~680 ≥355 ≥17 ≥40
Long and flat products; 2.5<t<3 510~680 ≥355 ≥18 ≥40
Long and flat products; 3≤t≤16 470~630 ≥355 ≥22 ≥40
Long and flat products; 16<t≤40 470~630 ≥345 ≥22 ≥40
Long and flat products; 40<t≤63 470~630 ≥335 ≥21 ≥40
Long and flat products; 63<t≤80 470~630 ≥325 ≥20 ≥40
Long and flat products; 80<t≤100 470~630 ≥315 ≥20 ≥40
Long and flat products; 100<t≤150 450~600 ≥295 ≥18 ≥40
Long and flat products; 150<t≤200 450~600 ≥285 ≥17 ≥33
Long and flat products; 200<t≤250 450~600 ≥275 ≥17 ≥33
Long products and flat products; 250<t≤400 450~600 ≥265 ≥17 ≥33
Approximate Comparison Table
Japan European Standard United Kingdom
JIS EN Numerical Grade BS EN/BS
SM520B S355K2
Fe510DD2①
S355K2G4①
1.0596 50EE
S355K2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!