Grade 17Cr3
Corresponding Standard DIN EN ISO 683-3-2019
Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
Classification Alloy Steel
17Cr3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.14 0.15 0.6 - - 0.7 -
Maximum Value 0.2 0.4 0.9 0.025 0.035 1 0.4
17Cr3 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
All product shapes Soft Annealing (+A) ≤174
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17210-1986
Grade
Germany W-Nr.
DIN EN 10084-2008
Grade
Germany W-Nr.
DIN EN ISO 683-3-2019
Grade
1 Approximate Comparison Table
China Taiwan, China Japan South Korea Germany France Russia United Kingdom
GB ISC CNS JIS KS DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
15CrH A20155 SCr415H SCr415H SCr415H 17Cr3 1.7016 17Cr3 15Х 17Cr3
(655M13)
2 Approximate Comparison Table structural alloy steel
China International Organization for Standardization Germany European Standard Russia United Kingdom
GB ISO DIN EN/DIN EN Numerical Grade GOST BS EN/BS
15CrH 17Cr3 17Cr3 17Cr3 1.7016 15KH 527M17

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!