Grade 20NiCrMo2-2
Corresponding Standard DIN EN ISO 683-3-2019
Heat-Treatable Steels,Alloy Steels and Free-Cutting Steels--Part 3: Case-Hardening Steels
Classification Alloy Steel
Properties Carburizing Ability
20NiCrMo2-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.17 0.15 0.65 - - 0.35 0.4 - 0.15
Maximum Value 0.23 0.4 0.95 0.025 0.035 0.7 0.7 0.4 0.25
20NiCrMo2-2 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
All product shapes Soft Annealing (+A) ≤212
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 161~212
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 149~194
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17210-1986
Grade
Germany W-Nr.
DIN EN 10084-2008
Grade
Germany W-Nr.
DIN EN ISO 683-3-2019
Grade
Approximate Comparison Table Hardenability Guaranteed Structural Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
20CrNiMoH A50205 SNCM220H SNCM220H SNCM220H 8620H H86200 20NiCrMo2H 20NiCrMo2-2 1.6523 20NiCrMo2-2 20ХГНМ 2506 (805H17)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!