Grade 20MoCr4
Germany W-Nr. 1.7321
Corresponding Standard DIN EN 10084-2008
Case hardening steels – Technical delivery conditions
Classification Alloy Steel
20MoCr4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.17 - 0.7 - - 0.3 0.4
Maximum Value 0.23 0.4 1 0.025 0.035 0.6 0.5
20MoCr4 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Semifinished products, bars Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤207
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 156~207
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 140~187
Approximate Comparison Table
China United States International Organization for Standardization Germany European Standard
GB ISC ASTM/AISI ISO DIN EN/DIN W-Nr. EN Numerical Grade
G20CrMo B10200 A534 4118H ≈20MnCrMo4-2
(B27)
20MoCr4
20MoCr4 1.7321 20MoCr4 1.7321

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!