Grade X12CrMnNiN 17-7-5
European Standard Steel Grade 1.4372
Corresponding Standard EN 10088-3-2014
Stainless steels-Part 3: Technical delivery condition for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 7.8 g/cm3
X12CrMnNiN 17-7-5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 5.5 - - 16 3.5 0.05
Maximum Value 0.15 1 7.5 0.045 0.015 18 5.5 0.25
X12CrMnNiN 17-7-5 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, rod, wire, section, bright products; d≤160 +AT 680~880 ≥230 (long.)
≥40
≤260 (long.)
≥100
Bar, rod, wire, section, bright products; 160<d≤250 +AT 680~880 ≥230 (tr.)
≥35
≤260 (tr.)
≥60
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization European Standard
GB ISC CNS JIS KS ASTM UNS ISO EN Numerical Grade
12Cr17Mn6Ni5N
(1Cr17Mn6Ni5N)
S35350 201 SUS 201 STS 201 201 S20100 X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
1.4372
1.4618
2 Approximate Comparison Table
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S35350 SUS201 S20100 X12CrMnNiN17-7-5 4372-201-00-I 1.4372
3 Approximate Comparison Table
Japan United States France European Standard
JIS ASTM NF EN/NF EN Numerical Grade
SUS201 201 Z12CMN17-07Az X12CrMnNiN17-7-5 1.4372

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!