Grade 18CrMo4
Corresponding Standard UNI 8550-1984
Specification unalloyed and alloyed steel finished products, open die and drop forged, for case hardening - Qualities, requirements and tests
Classification Alloy Steel
18CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.15 0.15 0.6 - - 0.85 0.15
Maximum Value 0.21 0.4 0.9 0.035 0.035 1.15 0.25
18CrMo4 Mechanical Properties
thickness/diameter
t/d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
d≤11 1130~1420 ≥880 ≥8 KCU
≥25
11<d≤25 835~1130 ≥590 ≥9 ≥30
25<d≤50 735~980 ≥540 ≥10 ≥30

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!