Grade 17Cr3
European Standard Steel Grade 1.7016
Corresponding Standard EN 10084-1998
Case hardening steels. Technical delivery conditions
Classification Alloy Steel
17Cr3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.14 - 0.6 - - 0.7
Maximum Value 0.2 0.4 0.9 0.035 0.035 1
1 Approximate Comparison Table
China Taiwan, China Japan South Korea Germany France Russia United Kingdom
GB ISC CNS JIS KS DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
15CrH A20155 SCr415H SCr415H SCr415H 17Cr3 1.7016 17Cr3 15Х 17Cr3
(655M13)
2 Approximate Comparison Table structural alloy steel
China International Organization for Standardization Germany European Standard Russia United Kingdom
GB ISO DIN EN/DIN EN Numerical Grade GOST BS EN/BS
15CrH 17Cr3 17Cr3 17Cr3 1.7016 15KH 527M17
3 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
17Cr3 17Cr3 1.7013

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!