Grade 00Cr17
Corresponding Standard Q/RP 006-2018
Cold Heading Stainless Steel Wire Rod
Brand/Supplier
-> Tsingshan Holding Group
Classification Ferritic Stainless Steel
00Cr17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value - - - - - 16 - - -
Maximum Value 0.03 1 1 0.04 0.03 18 0.6 0.25 0.6
00Cr17 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Coil: 700℃~820℃ Air Cooling or Rapid Cooling
Annealing + Pickling
400~520 ≥25 ≥55

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!