Grade 20Cr13
Corresponding Standard Q/RP 006-2018
Brand/Supplier
-> Tsingshan Holding Group
Classification Martensitic Stainless Steel
20Cr13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.16 - - - - 12 - -
Maximum Value 0.25 1 1 0.04 0.03 14 0.6 0.6
20Cr13 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Coil: 780°C~870°C Slow Cooling
Annealing + Pickling
≤180