Grade 07Cr19Ni10
China ISC S30409
Corresponding Standard GB /T 24511-2017
Stainless steel and heat resisting steel plate, sheet and strip for pressure equipments
Classification Austenitic Stainless Steel
Density 7.9 g/cm3
07Cr19Ni10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value 0.04 - - - - 18 8 -
Maximum Value 0.1 0.75 2 0.035 0.015 20 10.5 0.1
07Cr19Ni10 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: Solid Solution Treatment ≥520 Rp0.2:≥220
Rp1.0:≥250
≥40
HBW:≤201
HRB:≤92
HV:≤210
1 Approximate Comparison Table
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
07Cr19Ni10 S30409 SUS 304H 304H S30409 X6CrNi 18-10
X7CrNi 18-9
X6CrNi18-10 1.4948 X6CrNi18-10 1.4948
2 Approximate Comparison Table Seamless steel tubes and pipes for high pressure boiler
China United States European Standard
GB ISC ASTM/AISI EN
10Cr9MoW2VNbBN S30409 SA-213 TP304H X6CrNi18-10