Grade 07Cr17Ni12Mo2
China ISC S31609
Corresponding Standard GB /T 24511-2017
Stainless steel and heat resisting steel plate, sheet and strip for pressure equipments
Classification Austenitic Stainless Steel
Density 8 g/cm3
07Cr17Ni12Mo2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value 0.04 - - - - 16 10 2 -
Maximum Value 0.1 1 2 0.035 0.015 18 14 3 0.1
07Cr17Ni12Mo2 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: Solid Solution Treatment ≥515 Rp0.2:≥220 ① ≥40
HBW:≤217
HRB:≤95
HV:≤220
Approximate Comparison Table
China United States European Standard
GB ISC ASTM/AISI UNS EN Numerical Grade
07Cr17Ni12Mo2
(1Cr17Ni12Mo2)
S31609 316H S31609 X3CrNiMo 17-13-3 1.4436