Grade 06Cr17Ni12Mo2N
China ISC S31658
Corresponding Standard GB /T 24511-2017
Stainless steel and heat resisting steel plate, sheet and strip for pressure equipments
Classification Austenitic Stainless Steel
Density 8 g/cm3
06Cr17Ni12Mo2N Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16 10 2 0.1
Maximum Value 0.08 1 2 0.035 0.015 18 13 3 0.16
06Cr17Ni12Mo2N Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: Solid Solution Treatment ≥550 Rp0.2:≥240 ① ≥35
HBW:≤217
HRB:≤95
HV:≤220
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States Germany
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr.
06Cr17Ni12Mo2N
(0Cr17Ni12Mo2N)
S31658 316N SUS 316N STS 316N 316N S31651 X2CrMiMoN17-11-2 1.4406
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
GB ISC JIS UNS ISO Numerical Grade Numerical Grade
06Cr17Ni12Mo2N S31658 SUS316N S31651 X6CrNiMoN17-12-3 4495-316-51-J (1.4495)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!