Grade 06Cr18Ni11Ti
China ISC S32168
Corresponding Standard GB /T 24511-2017
Stainless steel and heat resisting steel plate, sheet and strip for pressure equipments
Classification Austenitic Stainless Steel
Density 8 g/cm3
06Cr18Ni11Ti Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Ti≥5C~0.7
Maximum Value 0.08 0.75 2 0.035 0.015 19 12
06Cr18Ni11Ti Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Steel: Solid Solution Treatment ≥520 Rp0.2:≥205
Rp1.0:≥250
≥40
HBW:≤217
HRB:≤95
HV:≤220
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Ti S32168 321 SUS 321 STS 321 321 S32100 X6CrNiTi 18-10 4541-321-00-I X6CrNiTi 18-10
(X10CrNiTi 18-9)
1.4541 Z6CNT 18-10 X6CrNiTi 18-10 1.4541 09Х18Н10Т
Х18Н10Т
2337 321S12
321S31
2 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr18Ni11Ti
(0Cr18Ni11Ti)
S32168 321 SUS 321 STS 321 321 S32100 X6CrNiTi 18-10 X6CrNiTi 18-10
(X10CrNiTi 18-9)
1.4541 Z6CNT 18-10 X6CrNiTi 18-10 1.4541 09Х18Н10Т 2337 321S12
321S31
3 Approximate Comparison Table Stainless steels for cold heading and cold extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
06Cr18Ni11Ti
(0Cr18Ni11Ti)
S32168 SUS321 321 S32100 X6CrNiTi18-10 4541-321-00-I X6CrNiTi18-10 1.4541

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!