Grade 12Cr16Ni35
China ISC S33010
Old Grade
Corresponding Standard GB /T 20878-2007
Stainless and heat-resisting steels - Designation and chemical composition
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 8 g/cm3
12Cr16Ni35 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 14 33
Maximum Value 0.15 1.5 2 0.04 0.03 17 37
1 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade BS EN/BS
12Cr16Ni35
(1Cr16Ni35)
S33010 SUH 330 SUH 330 STR 330 330 N08330 X12CrNiSi 35-16 X12NiCrSi 36-16 1.4864 Z12NCS 35-16
Z12NC 37-18
X12NiCrSi 35-16 1.4864 NA 17
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S33010 SUH330 X13NiCr35-16 4864-083-77-X 1.4864