Grade 17Cr3
European Standard Steel Grade 1.7016
Corresponding Standard EN 10132-2021
Cold Rolled Narrow Steel Strip for Heat Treatment - Technical Delivery Conditions
Classification Alloy Steel
17Cr3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.12 - 0.6 - - 0.7 -
Maximum Value 0.2 0.4 0.9 0.025 0.035 1.25 0.4
① Elements not quoted in this table shall not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions shall be taken to prevent the addition, from scrap or other material used in manufacture, of such elements which affect the hardenability, mechanical properties and application.
17Cr3 Mechanical Properties
Delivery condition* Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
annealed (+A) or annealed and skin passed(+LC) ≤550 ≤420 ≥21 HV
≤170
cold rolled(+CR) Agreed Upon at Time of Order Agreed Upon at Time of Order
• The elongation values in the table are for a gauge length of 80 mm.
• +A=annealed,+LC=annealed and skin passed,+CR=cold rolled,+QT=quenched and tempered
1 Approximate Comparison Table Hardenability Guaranteed Structural Steel
China Taiwan, China Japan South Korea Germany France Russia United Kingdom
GB ISC CNS JIS KS DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
15CrH A20155 SCr415H SCr415H SCr415H 17Cr3 1.7016 17Cr3 15Х 17Cr3
(655M13)
2 Approximate Comparison Table Structural Alloy Steel
China International Organization for Standardization Germany European Standard Russia United Kingdom
GB ISO DIN EN/DIN EN Numerical Grade GOST BS EN/BS
15CrH 17Cr3 17Cr3 17Cr3 1.7016 15KH 527M17
3 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
17Cr3 17Cr3 1.7013

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!