Grade S235JR
Germany W-Nr. 1.0037
Corresponding Standard DIN EN 10025-1994
Hot rolled products of non-alloyed structural steels Technical delivery conditions
Classification Carbon Steel
S235JR Chemical Element Composition Content (%)
  Component C Mn P S N
厚度t≤16 Minimum Value - - - - -
Maximum Value 0.17 1.4 0.045 0.045 0.009
  Component C Mn P S N
厚度16<t≤40 Minimum Value - - - - -
Maximum Value 0.2 1.4 0.045 0.045 0.009
S235JR Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t<3 360~510 ≥235 ≥21
3≤t≤16 340~470 ≥235 ≥26
16<t≤40 340~470 ≥225 ≥26
1 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST SS BS EN/BS
Q235A
Q235B
Q235C
Q235D
(A3)
(C3)
U12352
U12355
U12358
U12359
SS400 SS400
(SS41)
SS400 A570 Gr.A
A570 Gr.D
A283M Gr.D
K02501
K02502
Fe360A
Fe360D
S235JR
S235JRG1
S235JRG2
(St37-2)
(USt37-2)
(RSt37-2)
1.0037
1.0036
1.0038
S235JR
S235JRG1
S235JRG2
(E24-2)
(E24-2NE)
Ст3кп-2
Ст3кп-3
Ст3кп-4
БСт3кп-2
1311
1312
S235JR
S235JRG1
S235JRG2
(40B)
(C)
2 Approximate Comparison Table Construction Rebar
China Japan United States International Organization for Standardization Germany France Russia
GB ISC JIS ASTM ISO DIN EN/DIN NF EN/NF GOST
Q235 U12352 SR235 A570 Grade A PB240 S235JR FeE235 Ст3кп
Ст3пс
Ст3сп

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!