Grade
C20C
European Standard Steel Grade
1.0411
Corresponding Standard
EN 10263-2-2001
Steel Rod,bars and Wire for Cold Heading and Cold Extrusion - Part 2: Technical Delivery Conditions for Steels Not Intended for Heat Treatment after Cold Working
Classification
Carbon Steel
C20C Chemical Element Composition Content (%)
Component
C
Si ①
Mn ②
P
S
Al ③
Minimum Value
0.18
-
0.7
-
-
0.02
Maximum Value
0.22
0.1
0.9
0.025
0.025
0.06
C20C Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
5<d≤100
+U or +U+PE
≤560
≥55
5<d≤100
+AC or AC+PE
≤480
≥65
5<d≤10
+U+C
≤650
≥53
10<d≤40
+U+C
≤640
≥53
2<d≤5
+U+C+AC
≤470
≥67
5<d≤40
+U+C+AC
≤460
≥67
2<d≤5
+U+C+AC+LC
≤510
≥63
5<d≤40
+U+C+AC+LC
≤500
≥63
5<d≤10
+AC+C
≤570
≥60
10<d≤40
+AC+C
≤560
≥60
1 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
Japan
International Organization for Standardization
European Standard
JIS
ISO
EN
Numerical Grade
SWRCH22A
C20C
C20C
1.0411
2 Approximate Comparison Table
3 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
4 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
Japan
International Organization for Standardization
European Standard
JIS
ISO
EN
Numerical Grade
SWRCH22A
C20C
C20C
1.0411
5 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
C20C Corresponding Standards(Same grade name, different standards)